Any oil based prep product, rather than acrylic, as a base for a sealant may lessen durability, but the effect differs depending on the sealant. I did a 50/50 on a friends bonnet with Zymol HD Cleanse and SRP, both topped with Zaino Z2, and the durability from the SRP was noticeably better.
So, beyond the initial 'looks', I'd always recommend using something less oily than Lime Prime as a base for a sealant, based upon the above, and the general consensus from DW.
Oily base for a wax... acrylic/nothing for a sealant.
That said, a LOT of sealant will eat through whatever is on the car anyway to bond properly with the paint, so it could be that the Lime Prime layer is wasted anyway, unless used for correction, but then there are better products out there anyway...